Magnetocaloric Effect in a Microporous Material Using a Rare-Earth-Free, Hybrid Perovskite
来源 :ACS PublicationsMagnetic refrigeration using the magnetocaloric effect (MCE), where the temperature of a material changes as a magnetic field is applied, is a promising technology to increase the ...